Table 6

Material parameters using the Mooney–Rivlin hyperelastic material model that were derived experimentally by Tawk et al.

Material constantValue [unit]
C10−0.233 [MPa]
C012.562 [MPa]
C200.116 [MPa]
C11−0.561 [MPa]
C020.900 [MPa]
Incompressibility parameter D10.000 [MPa−1]