Influence of the injection method on the LMG material permeation
| LMG material | Coarse-grained material | Permeation: l | |||
|---|---|---|---|---|---|
| L/A = 1.4 | L/A = 1.7 | ||||
| D max: mm | d 15: mm | Method 1 | Method 2 | Method 1 | Method 2 |
| 2 | 35 | 0.2 | 2.9 | 2.3 | 25.0a |
| 2 | 75 | 1.7 | 13.4 | 6.9 | 24.3b |
| 2 | 110 | 2.4 | 25.1a | 19.0 | 25.1a |
| 4 | 35 | 0.6 | 3.3 | 5.9 | 25.5a |
| 4 | 75 | 3.5 | 20.0 | 21.4 | 25.0a |
| 4 | 110 | 16.2 | 24.5a | 25.1a | 25.3a |
| LMG material | Coarse-grained material | Permeation: l | |||
|---|---|---|---|---|---|
| L/A = 1.4 | L/A = 1.7 | ||||
| Method 1 | Method 2 | Method 1 | Method 2 | ||
| 2 | 35 | 0.2 | 2.9 | 2.3 | 25.0 |
| 2 | 75 | 1.7 | 13.4 | 6.9 | 24.3 |
| 2 | 110 | 2.4 | 25.1 | 19.0 | 25.1 |
| 4 | 35 | 0.6 | 3.3 | 5.9 | 25.5 |
| 4 | 75 | 3.5 | 20.0 | 21.4 | 25.0 |
| 4 | 110 | 16.2 | 24.5 | 25.1 | 25.3 |
No LMG material left in the cylindrical steel container
Some LMG material stuck on the inside wall of the cylindrical steel container
Note: consistency = 100 mm