Percentage reduction in vertical deformation for each experiment
| Moisture content | Test code | Vertical deformation corresponding to maximum vertical stress for compression of 50 mm in the control experiments: mm | Reduction in vertical deformation compared to the control tests: % |
|---|---|---|---|
| OMC | M1 (control – max. stress of 203 kPa) | — | — |
| M1-S | 24 | 52 | |
| M1-S-RF0.025% | 22 | 56 | |
| M1-S-RF0.05% | 21 | 58 | |
| M1-S-RF0.1% | 23 | 54 | |
| LL | M2 (control – max. stress of 30 kPa)) | — | — |
| M2-S | 29 | 42 | |
| M2-S-RF0.025% | 22 | 56 | |
| M2-S-RF0.05% | 15 | 70 | |
| M2-S-RF0.1% | 12 | 76 |
| Moisture content | Test code | Vertical deformation corresponding to maximum vertical stress for compression of 50 mm in the control experiments: mm | Reduction in vertical deformation compared to the control tests: % |
|---|---|---|---|
| OMC | M1 (control – max. stress of 203 kPa) | — | — |
| M1-S | 24 | 52 | |
| M1-S-RF0.025% | 22 | 56 | |
| M1-S-RF0.05% | 21 | 58 | |
| M1-S-RF0.1% | 23 | 54 | |
| LL | M2 (control – max. stress of 30 kPa)) | — | — |
| M2-S | 29 | 42 | |
| M2-S-RF0.025% | 22 | 56 | |
| M2-S-RF0.05% | 15 | 70 | |
| M2-S-RF0.1% | 12 | 76 |