Table 6

Cv values of specimens at different loading stresses

AdditiveCoefficient of consolidation, Cv: m2/year
25 kPa50 kPa100 kPa200 kPa400 kPa
S1S2S1S2S1S2S1S2S1S2
Untreated7.067.025.766.103.504.102.612.921.571.63
G10PA4.915.864.134.763.053.282.621.821.331.30
G20PA4.924.923.574.063.062.542.342.111.351.25
G30PA3.233.622.744.102.713.382.101.721.251.15
G40PA3.155.872.743.032.352.432.111.631.161.03