TCR values of pastes with various technology
| Paste | Firing atmosphere | Peak temperature[°C] | TCR [ppm/°C] |
|---|---|---|---|
| P1 | Air | 550 | −576 ± 22 |
| N2 | 875 | −676 ± 109 | |
| P1 overglaze | Air | 550/550 | −966 ± 25 (*) |
| N2 | 875/620 | −696 ± 86 (**) | |
| P2 | Air | 550 | −1,030 ± 14 |
| N2 | 875 | −1,060 ± 385 | |
| P2 overglaze | Air | 550/550 | −1,060 ± 12 (*) |
| N2 | 875/620 | −903 ± 21 (*) −490 ± 57 (***) |
| Firing atmosphere | Peak temperature[°C] | TCR [ppm/°C] | |
|---|---|---|---|
| Air | 550 | −576 ± 22 | |
| N2 | 875 | −676 ± 109 | |
| Air | 550/550 | −966 ± 25 ( | |
| N2 | 875/620 | −696 ± 86 ( | |
| Air | 550 | −1,030 ± 14 | |
| N2 | 875 | −1,060 ± 385 | |
| Air | 550/550 | −1,060 ± 12 ( | |
| N2 | 875/620 | −903 ± 21 ( |
Notes:
*Resistor layer printed twice;
**resistor layer printed three times;
***resistor layer printed four times