Fatigue life of hot-rolled 16Mn steel predicted by different models under two-stage load
| Loading mode | σ1/MPa | σ2/MPa | n1/105 | n2/105 | Predicted by different models | |||
|---|---|---|---|---|---|---|---|---|
| Miner model | The prediction model in GAO Huiying (2016) | Prediction model 1 | Prediction model 2 | |||||
| 1 | 394 | 345 | 0.0935 | 2.695 | 0.7701 | 0.6373 | 0.8897 | 0.8671 |
| 2 | 394 | 345 | 0.197 | 2.361 | 0.7977 | 0.6908 | 0.9147 | 0.8962 |
| 3 | 394 | 345 | 0.394 | 2.095 | 0.9422 | 0.8538 | 1.0544 | 1.0389 |
| 4 | 394 | 345 | 0.4675 | 1.593 | 0.8961 | 0.8377 | 0.9926 | 0.9822 |
| 5 | 394 | 345 | 0.561 | 0.740 | 0.7840 | 0.7633 | 0.8371 | 0.8332 |
| 6 | 345 | 394 | 1.810 | 0.828 | 1.3363 | 1.2657 | 1.2651 | 1.3990 |
| 7 | 345 | 394 | 1.971 | 0.809 | 1.3560 | 1.2757 | 1.2745 | 1.4196 |
| 8 | 345 | 394 | 2.333 | 0.595 | 1.2171 | 1.1123 | 1.1097 | 1.2793 |
| Loading mode | Predicted by different models | |||||||
|---|---|---|---|---|---|---|---|---|
| Miner model | The prediction model in | Prediction model 1 | Prediction model 2 | |||||
| 1 | 394 | 345 | 0.0935 | 2.695 | 0.7701 | 0.6373 | 0.8897 | 0.8671 |
| 2 | 394 | 345 | 0.197 | 2.361 | 0.7977 | 0.6908 | 0.9147 | 0.8962 |
| 3 | 394 | 345 | 0.394 | 2.095 | 0.9422 | 0.8538 | 1.0544 | 1.0389 |
| 4 | 394 | 345 | 0.4675 | 1.593 | 0.8961 | 0.8377 | 0.9926 | 0.9822 |
| 5 | 394 | 345 | 0.561 | 0.740 | 0.7840 | 0.7633 | 0.8371 | 0.8332 |
| 6 | 345 | 394 | 1.810 | 0.828 | 1.3363 | 1.2657 | 1.2651 | 1.3990 |
| 7 | 345 | 394 | 1.971 | 0.809 | 1.3560 | 1.2757 | 1.2745 | 1.4196 |
| 8 | 345 | 394 | 2.333 | 0.595 | 1.2171 | 1.1123 | 1.1097 | 1.2793 |