Static strength failure mode of composite/metal bolted joint
| Researcher | Composite | Metal | Joint | Failure mode |
|---|---|---|---|---|
| Zuo (2018) | T800/X850 3.384 mm | Ti6Al4V 3.4 mm*2 | Single nail and single shear | Extrusion and shear failure |
| Cao et al. (2018) | T800/X850 3.384 mm | Ti6Al4V 3.9 mm*2 | Single nail double shear | Extrusion failure |
| Liu et al. (2013b) | CYCOM977 3.8 mm | Ti6Al4V 2 mm | Double nail single shear | Extrusion failure |
| Li et al. (2019) | T700 3.2 mm | Al7075 3 mm | Single nail and single shear | Extrusion and shear failure |
| Kweon (2019) | USN125 1.5 mm*2 | 7075-T62 3.224 mm | Single nail double shear | Extrusion failure |
| Gui et al. (2021) | Composite | Aluminum alloy | Multiple nails and single scissors | Extrusion failure |
| Researcher | Composite | Metal | Joint | Failure mode |
|---|---|---|---|---|
| T800/X850 | Ti6Al4V | Single nail and single shear | Extrusion and shear failure | |
| T800/X850 | Ti6Al4V | Single nail double shear | Extrusion failure | |
| CYCOM977 | Ti6Al4V | Double nail single shear | Extrusion failure | |
| T700 | Al7075 | Single nail and single shear | Extrusion and shear failure | |
| USN125 | 7075-T62 | Single nail double shear | Extrusion failure | |
| Composite | Aluminum alloy | Multiple nails and single scissors | Extrusion failure |
Source(s): Table created by authors