Figure 3.
A graph displaying Raman spectroscopy results for different C Z T S samples, showing intensity on the vertical axis and Raman shift on the horizontal axis, with peaks labelled.This graphical representation illustrates Raman spectroscopy data for various Copper Zinc Tin Sulfide, C Z T S, samples, including labels for C Z T S A D, C Z T S 340, C Z T S 360, and C Z T S 380, indicated by distinct lines. The vertical axis denotes intensity, measured in arbitrary units, while the horizontal axis features Raman shift, indicated in centimetres inverse. A notable peak, associated with the A 1 mode vibration labelled C Z T S, reaches just over 1200 in intensity. The data suggests comparative analysis across the different samples, with the curves displaying peaks at differing Raman shifts, important for interpreting material properties.

Raman spectroscopy results of all CZTS thin film