Cyclic voltametry and potentiodynamic single sweep techniques are used to study the electrochemical behaviour of lead in Na2CO3 solutions containing various concentrations of ClO4‐ as aggressive anion. The effects of different concentrations, in terms of destruction of passivity and initiation of pitting corrosion, were monitored with reference to the change in integrated anodic charge. It was found that Δqa (taken as a measure of the extent of pitting) varies linearly with log CClO4‐. The pitting corrosion potential, Epitting, varies with log CClO4‐ according to sigmoidal curves. These curves are explained on the basis of formation of passive, active and continuously propagating pits. Additions of aliphatic amines shift the pitting corrosion potential, Epitting, into the noble (positive) direction, indicating the inhibition action of the added amines on the pitting attack. Epitting varies with the logarithm of the inhibitor concentration according to: Epitting = a + b log Cinh. The inhibition of pitting corrosion by the aliphatic amines is assumed to be due to either competitive adsorption between the CO32– with ClO4‐ anions, and/or the chemisorption of the amine on the metal with the formation of a metal‐nitrogen coordination bond. The efficiency of these compounds as pitting corrosion inhibitors increases with the increase in the chain length of the alkyl group.
Article navigation
1 April 2001
Editors
Review Article|
April 01 2001
Studies on the pitting corrosion of lead in carbonate media
E.E. Abd El Aal
E.E. Abd El Aal
Chemistry Department, Faculty of Science, Zagazig University, Zagazig, Egypt
Search for other works by this author on:
Publisher: Emerald Publishing
Online ISSN: 1758-4221
Print ISSN: 0003-5599
© MCB UP Limited
2001
Anti-Corrosion Methods and Materials (2001) 48 (2): 116–126.
Citation
Abd El Aal E (2001), "Studies on the pitting corrosion of lead in carbonate media". Anti-Corrosion Methods and Materials, Vol. 48 No. 2 pp. 116–126, doi: https://doi.org/10.1108/00035590110384119
Download citation file:
New and popular articles
Suggested Reading
Poly(4‐vinylpyridine) and poly(4‐vinylpyridine poly‐3‐oxide ethylene) as corrosion inhibitors for Cu60‐Zn40 in 0.5M HNO3
Anti-Corrosion Methods and Materials (October,2001)
A study of corrosion inhibition of carbon steel in hydrochloric acid by some benzene nitriles using the quantum chemistry calculation
Anti-Corrosion Methods and Materials (September,2007)
Inhibition of corrosion of copper by 5‐mercapto‐3‐p‐nitrophenyl‐1,2,4‐triazole in aqueous environment
Anti-Corrosion Methods and Materials (June,2001)
Quantitative relationships between the structure of some thiol compounds and their inhibition efficiencies
Anti-Corrosion Methods and Materials (June,2008)
The cyclic hydroxylamines: a new class of corrosion inhibitors of carbon steel in acidic medium
Anti-Corrosion Methods and Materials (June,2003)
Related Chapters
Fate and Transport of Lead Pollution Along a Highway Corridor
GEOENVIRONMENTAL ENGINEERING: Integrated management of groundwater and contaminated land
CORROSION INHIBITORS FOR SEVERE ENVIRONMENTS
Admixtures - Enhancing Concrete Performance: Proceedings of the International Conference held at the University of Dundee, Scotland, UK on 6 July 2005
Race, Environmental Inequality, and Physical Health
Underserved and Socially Disadvantaged Groups and Linkages with Health and Health Care Differentials
Recommended for you
These recommendations are informed by your reading behaviors and indicated interests.