In the production and overhaul of aero engines chemical and electrolytic surface treatment processes such as electrolytic degreasing, chemical and electrochemical etching, chemical descaling and chemical stripping of thermally sprayed coatings are used. In the course of some of these processes the heat resistant nickel and cobalt base alloys found in the “hot end” of the newer gas turbines are attacked. These superalloys have a common characteristic, namely, they are precipitation hardened. The alloying elements added for this purpose give rise to intermetallic compounds (carbides, nitrides, carbonitrides) which appear as inclusions of various shapes and sizes within the grain or at the grain boundaries. The conclusion from this work is that these intermetallics present as separate phases can be dissolved out by oxidative attack leaving pits. The separate processes and their objectives are detailed. It is shown in which process stages and in which solutions attack occurs. The inclusions have been analysed and the nature of the attack is illustrated. We conclude from this work, which has embraced seven nickel and cobalt base materials, that certain processes or process steps cannot be permitted on these alloys. For cleaning and etching alternative processes are given. For descaling a new compatible process was evaluated and will be discussed in a second report.
Article navigation
Review Article|
October 01 1981
Attack on superalloys by chemical and electrolytic processes
Publisher: Emerald Publishing
Online ISSN: 2059-9366
Print ISSN: 0002-2667
© MCB UP Limited
1981
Aircraft Engineering (1981) 53 (10): 22–25.
Citation
Simon H, Thoma M (1981), "Attack on superalloys by chemical and electrolytic processes". Aircraft Engineering, Vol. 53 No. 10 pp. 22–25, doi: https://doi.org/10.1108/eb035760
Download citation file:
247
Views
New and popular articles
Suggested Reading
Electrochemical study of nanocrystalline plasma electrolytic carbonitriding of CP‐Ti
Anti-Corrosion Methods and Materials (November,2007)
Chemical vibro‐descaling
Aircraft Engineering (November,1981)
Investigation into electrochemical machining of aviation grade inconel 625 super alloy: an experimental study with advanced optimization and microstructural analysis
Aircraft Engineering and Aerospace Technology: An International Journal (November,2024)
Research on the electrochemical dissolution behavior of Ni-based superalloys after different oxidation treatments in NaCl solution
Anti-Corrosion Methods and Materials (December,2024)
Investigation of silicon carbonitride/silicon for photoelectrochemical CO 2 reduction
Nanomaterials and Energy (September,2026)
Related Chapters
Efficacy of Electrolytic Generation and Transport of Oxygen for Soil Remediation
5th ICEG Environmental Geotechnics: Opportunities, Challenges and Responsibilities for Environmental Geotechnics: Proceedings of the ISSMGE’s fifth international congress organized by the Geoenvironmental Research Centre, Cardiff University and held at Cardiff City Hall on 26–30th June 2006
23. National project: nuclear steelmaking in Japan
The high temperature reactor and process applications
Preliminary test on modified clays for seawater resistant drilling
fluids
Geotechnical Engineering for Infrastructure and Development: XVI European Conference on Soil Mechanics and Geotechnical Engineering
Recommended for you
These recommendations are informed by your reading behaviors and indicated interests.