Skip to Main Content
Keywords: Anti-wear
Close
Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Industrial Lubrication and Tribology (2024) 76 (1): 1–10.
Published: 20 November 2023
... analyzed by X-ray photoelectron spectroscopy. Findings The addition of MoS2 can effectively improve friction-reducing and anti-wear action of the matrix, which is beneficial to form a lubricating film on the sliding track. After analyzing different changing mechanism of the sliding tracks...
Journal Articles
Industrial Lubrication and Tribology (2021) 73 (5): 830–838.
Published: 26 July 2021
.... The addition of antioxidants can reduce the consumption of ZDDP as an antioxidant, thus improving the anti-wear efficiency of ZDDP and reducing the excess phosphorus element in the grease. Design/methodology/approach In this study, an antioxidant with good comprehensive performance was selected from...
Journal Articles
Industrial Lubrication and Tribology (2020) 72 (8): 1013–1017.
Published: 24 February 2020
... for phosphate containing anti-wear layers. The purpose of this work is to investigate the influence of additive concentration and oil temperature on the formation of phosphate containing layers. Design/methodology/approach To investigate the formation of phosphate containing layers as a function...
Journal Articles
Industrial Lubrication and Tribology (2020) 72 (3): 439–447.
Published: 29 October 2019
... fabricated by laser texturing combined with hot-pressing. This paper showed that the lipophilicity of steel-hs was best among those of steel-s and steel-h. Babbitt alloy as a soft filler on dimples of steel substrate improved anti-wear of steel-s remarkably. It provides a new way...
Journal Articles
Industrial Lubrication and Tribology (2018) 70 (9): 1706–1713.
Published: 16 October 2018
... Publishing Limited 2018 Emerald Publishing Limited Licensed re-use rights only Coatings Epoxy resin Anti-wear Dry friction Anti-friction Friction mechanism Kevlar fibre Lubricant coating Tribological property Epoxy resin exhibits low curing shrinkage, stable chemical properties...
Journal Articles
Industrial Lubrication and Tribology (2018) 70 (9): 1684–1691.
Published: 08 October 2018
... the friction-reduced and anti-wear properties of paraffin oil, and Ag/RGO NCs has better tribological performance than Ag NPs. The excellent tribological properties were attributed to the special structure of Ag/RGO NC and the formation of tribofilm reducing the friction and wear on the shearing surfaces...
Journal Articles
Industrial Lubrication and Tribology (2017) 69 (6): 891–896.
Published: 13 November 2017
... lubricant additives with better oil-solubility. When the hindered phenol antioxidation functional group and alkyl-chain are introduced to thiadiazole, the resulting product could have better oil-solubility and excellent antioxidation resistance, anti-wear and corrosion resistance in the lubricating oil...
Journal Articles
Industrial Lubrication and Tribology (2015) 67 (2): 133–138.
Published: 09 March 2015
... formation across a broader set of conditions. Practical implications – Despite OSPs being polar and surface-active, they do not interfere with the ZDDP in forming an anti-wear film in a PAO and, therefore, their inherent properties of good deposit control could enhance the performance of modern...
Journal Articles
Industrial Lubrication and Tribology (2013) 65 (6): 466–471.
Published: 16 September 2013
...Weimin Li; Yanxia Wu; Xiaobo Wang; Weimin Liu Purpose – The purpose of this paper is to study the antirust, tribological performance and anti-wear (AW) mechanism of the of soybean lecithin (SL) as a kind of multifunctional lubricant additive. Design/methodology/approach – As a kind...
Journal Articles
Industrial Lubrication and Tribology (2013) 65 (4): 219–225.
Published: 14 June 2013
... liquids, the novel crown‐type phosphate ionic liquids prepared in the present work exhibit a more excellent antiwear ability for steel/Al2024 contact at different loads and frequencies. By the morphological analysis with SEM, less debris was observed in the worn surface lubricated with crown‐type...