Purpose

As known, the wire and arc additive manufacture technique can achieve stable process control, which is represented with periodic surface waviness, when using empirical methods or feedback control system. But it is usually a tedious work to further reduce it using trial and error method. The purpose of this paper is to unveil the formation mechanism of surface waviness and develop a method to diminish it.

Design/methodology/approach

Two forming mechanisms, wetting and spreading and remelting, are unveiled by cross-section observation. A discriminant is established to differentiate which mechanism is valid to dominate the forming process under the given process parameters.

Findings

Finally, a theoretical method is developed to optimize surface waviness, even forming a smooth surface by establishing a matching relation between heat input (line energy) and materials input (the ratio of wire feed speed to travel speed).

Originality/value

Formation mechanisms are revealed by observing cross-section morphology. A discriminant is established to differentiate which mechanism is valid to dominate the forming process under the given process parameters. A mathematical model is developed to optimize surface waviness, even forming a smooth surface through establishing a matching relation between heat input (line energy) and materials input (the ratio of wire feed speed to travel speed).

Licensed re-use rights only
You do not currently have access to this content.
Don't already have an account? Register

Purchased this content as a guest? Enter your email address to restore access.

Please enter valid email address.
Email address must be 94 characters or fewer.
Pay-Per-View Access
$41.00
Rental

or Create an Account

Close Modal
Close Modal