The importance of the quality of the plated‐through‐hole copper barrel in double‐sided and multilayer PCBs is considered with regard to the problem of voids and blowholes in the solder fillet. The thickness of the copper, and its integrity and adherence to the drilled surface define its ability to withstand the pressure burst of gas from the outgassing laminate during the few seconds of the thermal spike induced by the molten solder prior to solidification. The ability of copper electroplate to bridge over areas devoid of electroless copper and produce a barrel free of pinholes is shown to be crucial to this problem. In addition, the use of a nickel layer is shown to enhance greatly the impermeability of the barrel to the evolving gases.