The microstructure and performances of GH4169 nickel (Ni)-based alloy were studied after adding the elements rhenium (Re) and tungsten (W) and then conducting heat treatment. The alloy containing the element rhenium showed less δ phase after heat treatment. For both alloys containing the element tungsten and the GH4169 alloy without any element, the δ phase and rectangular carbide were all precipitated after the heat treatment. The creep rupture life of the alloy added with the element rhenium was higher than that of the alloy added with the element tungsten at a high temperature. When a mixture of 75% sodium sulfate (Na2SO4) and 25% sodium chloride (NaCl) was applied at 950°C under the same conditions, the thermal corrosion resistance of the nickel-based alloy containing rhenium was obviously better than that of the nickel-based alloy containing tungsten. The hot-corrosion resistance of the GH4169 alloy without adding any element was slightly better than that of the alloy with tungsten.

You do not currently have access to this content.
Don't already have an account? Register

Purchased this content as a guest? Enter your email address to restore access.

Pay-Per-View Access
$39.00
Rental

or Create an Account

Close Modal
Close Modal