Plastic ball grid array packages were aged for up to 2000 hours. Various solder ball pad metallurgies were studied and solder ball shear tests were conducted at a range of ageing times. The solder ball shear strength was found to decrease after an initial hardening stage. The deterioration of solder ball shear strength was found to be mainly caused by the formation of intermetallic compound layers, together with microstructural coarsening and diffusion related porosity at the interface. For the ball pad metallurgy, two distinct intermetallic compound layer structures were observed to have formed after ageing. Once two continuous intermetallic compound layers formed fracture tended to occur at their interface. For the ball pad metallurgies which do not form two continuous intermetallic compound layers, the shear strength still decreased, due to the coarsening of the microstructure, intermetallic particle formation and diffusion related porosity at the surface of the Ni3Sn4.

You do not currently have access to this content.
Don't already have an account? Register

Purchased this content as a guest? Enter your email address to restore access.

Pay-Per-View Access
$41.00
Rental

or Create an Account

Close subscription notice
Close access options